Cylinder re-boring is required after a seizure, excessive wear or overheating. Metal is removed to ensure the cylinder is both round and parallel throughout its length. Over sized pistons are then required to take up the difference that the boring created. Pistons are usually but not always available in the following sizes: Standard (std) +.25mm, +.5mm, +.75mm +1mm. If your cylinder block is damaged or worn beyond the oversize available for your engine then the block will require re-sleeving or linering back to standard size or a size that a suitable piston is available.

Cylinder showing signs of corrosion & wear. Re-bore required. Freshly re-bored  cylinder to clearance size. Round & true.

Our Air-Floating Boring machine in action

Piston diameter in mm, measured at the point of greatest skirt diameter perpendicular to pin axis

The fitting clearance in mm.       “SP”= Spiel = Clearance In this example 0.10mm

Manufacturers Mark & Quality Symbol

Oversize indication. “STD” = Standard Or in this example .060” = +60 thou Oversize

Piston Catalogue Modified Flange Liners  fitted to a Rover V8

Liner fitting can be used to repair cracked or porous cylinder blocks.

Cylinder Boring. Re-Linering. Honing.

We always “Plateau” hone our re-bored cylinders. This is the final honing process which removes high peaks and normalises the cylinder bore finish. This is essential for more modern engine designs as the piston ring equipment is usually much finer

A popular modification for Volkswagen Air cooled engines is increased capacity.

This is achieved by fitting larger barrels with increased bore size and bigger pistons.

This modification requires the aluminium/magnesium crank case and cylinder head recess to be machined. We do this on our CNC milling machine as seen here.

This Volkswagen 5-cylinder engine is equipped with “nikasil” coated cylinders. This method allows the piston to work directly with the aluminium cylinder wall with the hard protective nikasil coating in between. The problem is that the coating is very thin and therefore very unforgiving. The slightest amount of piston pick up or cylinder distortion will destroy the thin coating and wear very very quickly. Even a faulty fuel injector can destroy the nikasil coating. We can repair these type of engines by removing the nikasil coating completely, boring the aluminium and fitting either a stepped or flanged cylinder liner. The original pistons can be reused if they have not worn or been damaged but a new set of piston rings will be required. The cylinder block seen here has been modified as described.

While your cylinder block is out of the car and stripped for re-boring it is a good idea to remove all of the core plugs and clean out all the sludge that has accumulated inside the water jacket. Over the years these deposits compromise the cooling systems capability. The core plugs can also corrode through from the inside and at this stage they will be easy to change. A wide range of both cup and dish type core plugs are in stock.


When re-linering  it is also important to clean out cooling aids like slots and passages as they become visible with the old liners removed. Failure to do so may cause overheating and seizure issues in the future.


Oil galleries and passages should also be thoroughly cleaned out at this stage.

Re-boring a cylinder block or cylinder liner is just the start. Although the boring procedure removes all the wear and makes the cylinder more uniform the process will leave the cylinder surface rough if viewed under a microscope. This rough surface finish would be bad for the piston rings and accelerated wear poor oil consumption and increased temperature would result. The piston rings would not seal correctly and cylinder compression and performance would be lost. This is why we finish the cylinder resizing process by honing. We carry out cylinder honing on a dedicated honing machine. Its a “Sunnen Cylinder King” manufactured in the USA. It uses abrasive stones and guide shoes that run directly in the cylinder and remove all the high peaks and torn metal that the boring machine leaves behind. This normalises the cylinder bore finish and makes it uniform without taper or ovality. Measurements a re continually taken during this process to ensure the correct piston to bore clearance is achieved.

Our Cylinder Honing Machine in Action.

Click here to view video

Here is a video where you can see our honing machine in action. Notice the large volume of cutting oil used directly on the honing head to flush away worn stones and bore material while cooling the cylinder preventing distortion. The clicking noise you can hear is the automatic feed maintaining stone pressure against the cylinder. The stroking mechanism can be interrupted to dwell at the bottom of the cylinder to maintain correct geometry.

1st stage roughing is done with a 120 grit stone set.

2nd stage finish & size is carried out using a 220 grit stone set. This suits most applications using cast iron cylinders which are then finished using cork or a plateau honing brush set.

3rd stage ultra fine 400+ grit stones can be used for special & race applications before plateau honing with a special brush set.

These are diamond  honing stones for stock removal and roughing.  These stones allow us to hone rather than bore. This saves on setup time and speeds up the process. Although these stones allow for any amount of material removal we usually use them for the removal of around 0.5mm and up.

These are new 220 grit finishing stones. We would generally remove the final  0.1mm with these stones as we approach the final bore size.

These are the honing guides. They ensure that the honing head is held parallel inside the cylinder bore while honing round and true. The shorter guides are used for long cylinder lengths.

VW Air cooled overbore machining

Click here to view video

Re-Boring Cylinder Re-Boring Piston Crown Markings Cylinder Liners Cylinder Honing Honing Procedure Nikasil Cylinders Air Cooled